17-4 H1150
stainless steel suppliers
Global Leader in Specialty Metals
My Account
Customer Login
Quote/Buy
Chat Now!
My Account
Open Quotes
Open Orders
Shipped Orders
Shipment Tracking
Material Test Reports
My Reports
Profile Change
Create a New Quote
View Current Quote
Feedback
Our Company
About Us
Locations
Quality Approvals
Packaging Requirements
MSDS
FAQs
Alloys
Nickel Alloys
RA330®
601
718 NACE
AL-6XN®
230®
RA333®
625
X
800H/AT
X-750
RA 602 CA®
718
INVAR 36
Alloy 20
W
600
Duplex Stainless Steels
ZERON® 100
ZERON® 100 FG
2205
LDX 2101®
Stainless Steels
RA 253 MA®
17-4 H1150
316 / 316L
317L
Prodec® 316/316L
309
17-4 HH1150
410
303
15-5
310
A-286
410S
303 HST
13-8
321
304 / 304H
446
Prodec® 303
Nitronic® 50
347
304 / 304L
455
Prodec® 304/304L
Nitronic® 60
17-4
Titanium Alloys
6Al-4V
6Al-4V ELI
6Al-4V STA
6Al-2Sn-4Zr-2Mo
10V-2Fe-3Al
Cobalt Alloys
188
René 41
C263
694
TRIBALOY® T-800®
L605
WASPALOY®
Special Offers
Processing
Laser Cutting
Waterjet Cutting
Coil Leveling
Abrasive Saw Cutting
Plasma Cutting
Hi-Def Plasma Cutting
Plate Beveling
Shear Cutting
Gauer
Straightener
Bar Saws
Pipe Beveling
Pipe Threading
Rod Coil Line
Technical Resources
Environments
Alloy Performance Guide
Corrosion Tables
Ferric Chloride
Hydrofluoric Acid
Phosphoric Acid
Caustic
Hydrochloric Acid
Nitric Acid
Sulfuric Acid
Oxidation
Sulfidation
Carburization
Molten Salts
Molten Metals
Fabrication
Welding
Forming
Machining
Tolerances
Technical Papers
Heat Resistant Alloys
Corrosion Resistant Alloys
Case Histories
RA330®
RA333®
RA 602 CA®
AL-6XN®
ZERON® 100
LDX 2101®
RA 253 MA®
316 / 316L
Prodec® 316/316L
Markets
Aerospace
Chemical Processing
Medical
Oil and Gas
Power Generation
Thermal Processing
In the News
Contact Us
Home
Alloys
Stainless Steels
17 4-H1150
800-521-0332
onlinesales@rolledalloys.com
Chat Now!
17-4 H1150
Product Information
Request A Quote
Jump To
17-4 H1150 Chemistry
Markets
Medical
Oil and Gas
17-4 H1150
Chemistry
Ni
Cr
Mo
Mn
Cu
Si
C
Cb+Ta
S
P
Fe
MIN
3.0
15.0
-
-
3.0
-
-
5 x C
-
-
-
MAX
5.0
17.5
0.05
1.0
4.0
1.0
0.07
0.45
0.03*
0.04*
Balance
*0.025 max, AMS 5622