Product Line
Inventory
Plate Sheet Bar Welding Products Forged Billet
Specifications
UNSW.Nr. Form ASME ASTM AMS CUSTOMER
R50550 Plate, sheet, strip SB-265 B 265 4900
3.7055 T-9046