LDX 2101
l
Corrosion Resistant Alloys
l
Product Line
LDX 2101 is a lean duplex stainless steel designed for general-purpose use. Like other duplex stainless steels LDX 2101 provides high strength and excellent resistance to chloride stress corrosion cracking. LDX 2101 is an economical alternative to Types 304L and 316L stainless steels.