188 is a cobalt base superalloy with a unique combination of high temperature strength and oxidation resistance, along with adequate ductility after prolonged exposure to the 1400-1600°F temperature range.  188 alloy is readily fabricated, being welded by both manual and automatic methods including electron beam, gas tungsten arc and resistance welding.