RA2205
l
Corrosion Resistant Alloys
l
Product Line
RA2205 is a duplex stainless steel that was developed as a cost effective solution to common corrosion problems encountered with 300 series stainless steels. The duplex structure of RA2205 gives it significantly higher strength than 316L stainless. As a result, lighter gages of RA2205 can often be utilized creating weight savings without sacrificing structural strength.