RA310 is an austenitic heat resisting alloy with excellent resistance to oxidation under mildly cyclic conditions to 2100°F. Rapid thermal cycling increases the rate of metal wastage somewhat by spalling of the protective oxide scale. The oxidation resistance of RA310 is significantly better than that of RA309.