RA321
l
Heat Resistant Alloys
l
Product Line
RA321 stainless is a titanium stabilized grade commonly used for a service in the 1000-1600°F (540-870°C) temperature range. For service temperatures up to about 1600°F (870°C), a stabilizing treatment at 1550-1650°F (840- 900°C), air cool, may be used to provide optimum resistance to intergranular corrosion and to polythionic acid stress corrosion cracking. RA321 is readily welded by all common methods including submerged arc.