Logo Home Login

RA333 l Heat Resistant Alloys l Product Line

RA333 is a high chromium nickel base superalloy with outstanding resistance to high temperature oxidation, carburization, and thermal shock.  In a gas fired application, RA333 alloy has been heated as high as the incipient melting point with no significant metal loss from oxidation.  RA333 is one of the few materials that can withstand corrosive conditions ranging from aqueous to white heat.  The alloy has been used for dampers and refractory anchors in 13% SO2/SO3 at 1800°F, and for refinery flare tips.  Upon shut-down, RA333 resists attack by sulfuric and polythionic acids formed below the dew point.  RA333 has exceptional resistance to molten glass and has replaced platinum spinnerets in the manufacture of fiberglass.

Specification Inventory
UNS DIN Form ASME ASTM AMS Plate Sheet Bar Pipe   Welding Products Forging Billet
N06333



W86333
2.4608 Plate, sheet, strip
Bar
Weld wire

Covered electrodes
B 718
B 719
5593
5717

  •  VIEW RA333 DATA SHEET   FABRICATION INFORMATION   CASE HISTORY   GET A QUOTE ON RA333 


    Privacy Policy Contact Webmaster Terms Conditions Copyright ISO 2002