RA446 is a high chromium ferritic heat resisting alloy with excellent resistance to oxidation and to various forms of hot corrosion. The RA446 alloy is most commonly used for service between 1500 and 2200°F (815 and 1200°C), although its elevated temperature strength is quite low.