RA600 is a nickel-base alloy with excellent carburization, and good oxidation resistance at elevated temperatures.  The alloy has long been used in the heat treating industry for many of the same applications as RA330.  RA600 has useful resistance to dry Cl2 and HCl gases at moderately elevated temperatures.  RA600 is not suggested for use at red heat when sulfur is present.

Specification Inventory
UNS DIN Form ASME ASTM AMS Plate Sheet Bar Pipe   Welding
Products
Forging
Billet
N06600 2.4816 Plate, sheet, strip
Rod, bar and wire
Weld wire
Covered electrodes
SB-168
SB-166
(AWS-ERNiCr-3)
(AWS-ENiCrFe-3)
B 168
B 166
5540
5665

  •  VIEW RA600 DATA SHEET   FABRICATION INFORMATION   GET A QUOTE ON RA600 