RA601 is a nickel-chromium alloy, highly resistant to oxidation through 2200°F. RA601 develops a tightly adherent oxide scale which resists spalling even under conditions of severe thermal cycling. The alloy has good high temperature strength, and retains its ductility after long service exposure. RA601 has good hot corrosion resistance under oxidizing conditions.
Specification
Inventory
UNS
DIN
Form
ASME
ASTM
AMS
Plate
Sheet
Bar
Pipe
Welding Products
Forging Billet
N06601
2.4851
Plate, sheet, strip
Seamless pipe
SB-168
SB-167
B 168
B 167
5870