718 l High Temperature Aerospace Alloys l Product Line

718 alloy is a high strength nickel base superalloy used from cryogenic temperatures up to long term service at 1200°F.  The 718 alloy is readily fabricated and may be welded in either the annealed or precipitation (age) hardened condition.