RA800H/AT
l
Heat Resistant Alloys
l
Product Line
RA800H/AT is an austenitic heat resistant alloy meant for high temperature structural applications. The strength of RA800H/AT is achieved by controlled levels of carbon, aluminum and titanium along with a 2100°F (1149°C) minimum anneal to achieve grain size ASTM 5 or coarser.
Specification
Inventory
UNS
DIN
Form
ASME
ASTM
AMS
Plate
Sheet
Bar
Pipe
WeldingProducts
Forging Billet
N08811
1.4876
Plate, sheet
Weld Wire
SB-409
(AWS-ERNiCr-3)
B 409
VIEW RA800H/AT DATA SHEET
FABRICATION INFORMATION
GET A QUOTE ON RA800H/AT