Alloy X is one of the most widely used nickel base superalloys for gas turbine engine components.  This solid solution strengthened grade has good strength and excellent oxidation resistance beyond 2000°F.  Alloy X has excellent resistance to reducing or carburizing atmospheres, making it suitable for furnace components.