321 stainless is a titanium stabilized grade commonly used for a service in the 1000-1600°F (540-870°C) temperature range. 321 is readily welded by all common methods including submerged arc.
Inventory
Plate Sheet Bar Welding
Check Check Check
Specifications
UNS Form AMS DIN G.E. PWA QQ-S ASME ASTM
S32100 Sheet 5510 1.4541 SA-240 A 240
Plate
Bar 5645 SA-479 A 479