17-4 is an age-hardening martensitic alloy combining high strength with the corrosion resistance of stainless steel. Hardening is achieved by a short-time, simple low-temperature treatment. Unlike conventional martensitic stainless steels, such as type 410, RA17-4 is quite weldable. The strength, corrosion resistance and simplified fabrication can make RA17-4 a cost-effective replacement for high strength carbon steels as well as other stainless grades.
Inventory
Plate Sheet Bar Welding
Specifications
UNS Form AMS DIN G.E. PWA QQ-S ASME ASTM
Wire 5825
Plate 5604 1.4548 SA-693 A 693
Bar 5643 SA-564 A 564