Tribaloy ® T-800
l
High Temperature Aerospace Alloys
l
Product Line
T-800 is a cobalt-chromium molybdenum alloy which inhibits galling between sliding surfaces where lubrication is difficult. The microstructure of alloy T- 800 consists of about 50% of the hard intermetallic Laves phase dispersed in a softer cobalt alloy matrix. This provides the material with exceptional metal to metal wear bearing properties.