Alloy C263 is an aluminum-titanium age hardening nickel base superalloy welding wire. Gas tungsten arc welding is normally carried out using argon shielding gas. Argon +5% hydrogen has been used. Alloy C263 base metal is normally welded in the annealed condition 2100°F, rapid cool). After welding, the assembly may be aged 8 hours at 1470°F, air cool. Repair welding of alloy C263 components may be done in the age hardened condition.
Cobalt 263
C263 Welding Products
UNS N07263, Werkstoff 2.4650, Nr./EN 2.4650, AMS 5966, GE B50A783, RR 9500/16
| Cr | Ni | Mo | Co | Al | Ti | Al+Ti | B | C | Fe | Mn | Si | P | S | Ag | Bi | Pb | Cu | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| MIN | 19 | 5.6 | 19.0 | 0.3 | 1.9 | 2.4 | - | 0.01 | - | - | - | - | - | - | - | - | - | |
| MAX | 21.00 | Balance | 6.10 | 21.00 | 0.60 | 2.40 | 2.80 | 0.005 | 0.08 | 0.70 | 0.60 | 0.40 | 0.015 | 0.007 | 0.0005 | 0.0001 | 0.002 | 0.20 |
Density: 0.302 lb/in3
Melting Range: 2372-2471°F
| Temperature, °F | 400 | 800 | 1000 | 1200 | 1400 | 1600 | 1800 |
| Coefficient* of Thermal Expansion, in/in°F x 10-6 |
6.7 | 7.4 | 7.7 | 8.1 | 8.7 | 9.6 | 10.2 |
* 70°F to indicated temperature.