| ZERON® 100 |
- |
S32760 A911SA 1.4501 |
25 |
7.0 |
3.5 |
0.25 |
62 |
0.7 Cu, 0.5 Mn, 0.22 N, 0.02 C, 0.7 W |
A highly alloyed super duplex stainless steel for use in seawater desalination and many aggressive environments. Minimum PREN of 40. |
| ZERON® 100 FG |
|
S32760 1.4501 |
25 |
7.0 |
3.5 |
0.25 |
62 |
0.7 Cu, 0.5 Mn, 0.22 N, 0.02 C, 0.7 W |
Strain hardened version of ZERON 100 in round bar for high strength marine fastener applications. |
| 2205 |
- |
S32205 S31803 1.4462 |
22.1 |
5.6 |
3.1 |
0.45 |
67 |
0.16 N |
Duplex stainless steel with high resistance to chloride attack. |
| LDX 2101® |
- |
S32101 1.4162 |
21.5 |
1.5 |
0.3 |
0.7 |
70 |
5.0 Mn, 0.22 N, 0.03 C |
A lean duplex stainless steel offering excellent strength, SCC resistance and economy. |