Alloy 625 is used both for its high strength and outstanding aqueous corrosion resistance. The strength of alloy 625 is primarily a solid solution effect from molybdenum and columbium. Alloy 625 has excellent weldability and is frequently used to weld AL-6XN® alloy. Matching filler metals are also used to join dissimilar metals.

Specifications

UNS N06625, Werkstoff 2.4856, EN 2.4856

ASTM B 443 Gr 1, ASTM B 446 Gr 1

ASME SB-443 Gr 1, ASME SB-446 Gr 1, ASME SFA-5.14, ASME Sect. IX P No. 43

NACE MR0175-3, ISO 15156-3

AMS 5599, ASM 5666, ASM 5837


Inventory

Alloy 625 Plate, Alloy 625 Sheet, Alloy 625 Coil, Alloy 625 Bar, Alloy 625 Welding Products

Common Trade Names

Inconel 625, Alloy 625, Nickel 625 

Chemical Composition, %

  Cr Ni Mo Co Cb+Ta Al Ti C Fe Mn Si P S
MIN 20.0 - 8.0 - 3.15 - - - - - - - -
MAX 23.0 Balance 10.0 1.0 4.15 0.4 0.4 0.1 5.0 0.5 0.5 0.015 0.015

Features

  • High creep-rupture strength
  • Oxidation resistant to 1800°F
  • Good fatigue resistance
  • Excellent weldability
  • Outstanding resistance to chloride pitting and crevice corrosion
  • Immune to chloride ion stress corrosion cracking
  • Resistant to seawater under both flowing and stagnant conditions and under fouling

Applications

  • Aircraft ducting systems
  • Jet engine exhaust systems
  • Engine thrust-reverser systems
  • Bellows and expansion joints
  • Turbine shroud rings
  • Flare stacks
  • Seawater components
  • Chemical process equipment handling mixed acids both oxidizing and reducing.

Physical Properties

Density: 0.305 lb/in3
Melting Point: 2350-2460°F

Temperature, °F 70 400 600 800 1000 1200 1400 1600
Coefficient* of Thermal Expansion, in/in°F x 10-6 - 7.3 7.4 7.6 7.8 8.2 8.5 8.8
Thermal Conductivity
Btu • ft/ft2 • hr • °F
5.7 7.2 8.2 9.1 10.1 11.0 12.0 13.2
Modulus of Elasticity, Dynamic psi x 106 30 28 28 27 26 24 23 -

* 70°F to indicated temperature.

Mechanical Properties

Representative Tensile Properties, Bar

Temperature,°F 70 400 600 800 1000 1200 1400 1600
Ultimate Tensile Strength, ksi 144 134 132 132 130 119 78 40
0.2% Yield Strength, ksi 84 66 63 61 61 60 59 39
Elongation, % 44 45 42.5 45 48 34 59 117

Typical Rupture Strength Bar, Stress to Rupture at Indicated Time

Temperature, °F 1200 1300 1400
100 Hours, ksi 59 34 18
1,000 Hours, ksi 43 23 12