Nominal Chemical Composition
Alloy AMS UNS/W.Nr. Cr Ni Mo Si Fe Other Description
ZERON® 100 - S32760 A911SA 1.4501 25 7.0 3.5 0.25 62 0.7 Cu, 0.5 Mn, 0.22 N, 0.02 C, 0.7 W A highly alloyed super duplex stainless steel for use in seawater desalination and many aggressive environments. Minimum PREN of 40.
ZERON® 100 FG S32760 1.4501 25 7.0 3.5 0.25 62 0.7 Cu, 0.5 Mn, 0.22 N, 0.02 C, 0.7 W Strain hardened version of ZERON 100 in round bar for high strength marine fastener applications.