Titanium Alloys

Nominal Chemical Composition
Alloy AMS UNS/W.Nr. Al V O2 Fe Ti Other Description
6Al-4V 4911
4928
4967
4920
4934
4935
T-9046
T-9047
R56400 3.7164 6.0 4.0 0.16 0.15 89.4 - Most widely used of all of the alpha-beta titanium alloys. Used through 750°F.
6Al-4V ELI 4905
4907
4930
4931
T-9046
R56401 6.0 4.0 0.1 0.15 89 - Extra low interstitial version of 6-4 Grade to maximize toughness. Commonly used for medical implants.
6Al-4V STA 4965
6930
T-9047
R56400 6.0 4.0 0.16 0.15 89.4 - The STA process increases the strength level, lowers the ductility and generally provides greater stability to the material.
6Al-2Sn-4Zr-2Mo 4919
4975
4976
T-9046
T-9047
R54620 6.0 - - - 86 2.0 Sn, 4.0 Zr A near-alpha alloy, primarily used for high strength and toughness, with good creep resistance up to 1000°F. Forging/Machining characteristics similar to those of Ti 6-4.
10V-2Fe-3Al 4983
4984
4986
4987
BMS 7-260M
R56410 3.2 9.3 0.1 1.8 85 - A near beta alloy developed as a high strength forging alloy.