- (2012 - Rolled Alloys)Selecting the Alloy
- (2010 - Industrial Heating)Micro-Alloyed Heat-Resistant Alloy Reduces Costs, Not Performance
- (2008 - Stainless Steel World)Heat Resistant Alloys Selection and Failure Avoidance
- (2008 - Industrial Heating)Heat-Resistant Alloy Selection - The Importance of Microstructure Under Cycling Conditions
- (2007 - Industrial Heating)Understanding Various Factors that Reduce Heat-Resistant-Alloy Component Life
- (2005 - NACE)Micro-Alloying Improves Resistance to High Temperature Environments
- (2005 - NACE)Case Histories on Successful Applications of Alloy RA 602CA UNS N06025 in High Temperature Environments
- (2005 - NACE & Heat Processing)Materials Selection Considerations for Thermal Process Equipment
- (2004 - NACE)Performance of Alloy RA 353 MA (UNS S35315) In Fossil Fuel Fired Applications
- (2002 - NACE)Combatting High Temperature Corrosion with Alloy RA 602CA (UNS N06025) in Various Environments and Industries
- (2002 - Industrial Heating)Nickel-Base Furnace Alloy Extends Maximum-Use Temperature
- (1997 - ASM Heat Treat Show)Wrought Heat Resisting Alloys Provide Cost Reductions
- (1999 - Stainless Steel World)Metal Dusting in the Heat Treating Industry
- (1995 - ASM International)Oxidation Rates of Some Heat Resistant Alloys
- (1993 - Heat Treating)Heat Resistant Alloy Performance
- (1992 - Industrial Heating)Influence of Composition and Microstructure on Performance of Wrought Heat Resisting Alloys
- (1990 - Heat Treating)Neutral Salt Pot Alloy Life Maintenance is the Key
- (1990 - NACE)The Use of New Generation Stainless Steels in combustion Systems
- (1986 - NACE)Evaluation of Heat Resistant Alloys in Composite Fixtures
- (1982 - Metal Progress)An Evaluation of Heat Resistant Alloy Furnace Components
- (1982 - Heat Treating)How Alloy Selection Figures in Design of Radiant Tubes
- (1979 - Industrial Heating)Understanding Conditions that Affect Performance of Heat Resisting Alloys
- (1974 - Metal Treating Magazine)Wrought Heat Resisting Alloys Provide Cost Reduction
- (1973 - Metal Progress)Analyzing Belt Pin Failures
- (1963 - Production Equipment Magazine)Lower Cost Heat Treating
- (1962 - )Cracking in Type 309 High Temperature Fabrications and How to Combat
- (1995 - Steel Magazine)Added Life for Brazing Fixtures