AL-6XN alloy is a superaustenitic stainless with outstanding resistance to chloride pitting and crevice corrosion. The levels of chromium, molybdenum and nitrogen all serve to provide the AL-6XN alloy with resistance to acidic, oxidizing chloride solutions previously achieved only by the nickel base alloys. High nickel (24%) and molybdenum (6.3%) contents make AL-6XN a useful engineering solution to the problem of chloride ion stress corrosion cracking.
Specifications
| N08367 |
|
Plate, sheet, strip |
SB-688 |
B 688 |
|
|
|
Welded pipe |
SB-675 |
B 675 |
|
|
|
Welded tube |
SB-676 |
B 676 |
|
|
|
Welded pipe, filler added |
-- |
B 804 |
|
|
|
Rod, bar, wire |
SB-691 |
B 691 |
|
|
|
Forged flanges, fittings |
SB-462 |
B 462 |
|
|
|
Nickel alloy forgings |
SB-564 |
B 564 |
|
|
|
Wrought welded fittings |
SB-366 |
B 366 |
|
|
|
Bar and billet for reforging |
-- |
B 472 |
|
|
|
Weld wire |
(AWS-ERNiCrMo-3) |
|
|
|
|
Covered electrodes |
(AWS-ENiCrMo-3) |
|
|