Technical Resource Center
RA 253 MA is a lean austenitic heat resistant alloy with high strength and outstanding oxidation resistance. RA 253 MA obtains its heat resistant properties by advanced control of micro alloy additions. The use of rare earth metals in combination with silicon gives superior oxidation resistance to 2000°F (1090°C). Nitrogen, carbon, and a dispersion of rare earth and alkaline earth oxides combine to provide creep rupture strength comparable to the nickel alloys.
Inventory
Plate Sheet Bar Pipe Welding Products Forging Billet
Check Check Check Check Check
Specifications
UNS DIN Form ASME ASTM AMS
S30815 1.4893 Plate, sheet, strip SA-240 A 240
EN 1.4835 Seamless, welded pipe
Bar
W30816 Weld wire