RA330 is an austenitic heat and corrosion resisting alloy offering an exceptional combination of strength and resistance to carburization, oxidation and thermal shock. Carburization and oxidation resistance to 2200°F are enhanced by a nominal 1.25% silicon addition. RA330 finds wide applications in high temperature industrial environments where good resistance to the combined effects of carburization and thermal cycling is a prime requisite. RA 330 remains fully austenitic at all temperatures and is not subject to embrittlement from sigma formation.
Specifications
| N08330 |
EN 1.4886 |
Plate, sheet, strip |
B 536 |
SB-536 |
5592 |
|
|
Bars and shapes |
B 511 |
SB-511 |
5716 |
|
|
Seamless pipe, tube |
SB-535 |
B 535 |
|
|
|
X-Metal, fasteners |
|
|
|
| N08334 |
|
Weld wire |
|
|
|
| W88334 |
|
Covered electrodes |
|
|
|