2507 is a super duplex stainless steel providing very high strength and corrosion resistance, superior to 2205 and approaching that of some nickel alloys.
Inventory
Plate Sheet Bar Pipe Welding Products Forging Billet
Check
Specifications
UNS DIN Form ASME ASTM AMS
S32750 1.4410 Plate SA-240 A240