AMS 4930

Titanium Alloy Bars, Wire, Forgings, and Rings, 6Al - 4V, Extra Low Interstitial, Annealed

This specification covers a titanium alloy in the form of bars, wire, forgings, flash welded rings, and stock for forging or flash welded rings.