AMS 5592

Iron-Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate, 44Fe - 18.5Cr - 35Ni - 1.15Si, Solution Heat Treated.

This specification covers a corrosion and heat-resistant iron-nickel alloy in the form of sheet, strip, and plate.