AMS 5598

Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate, 72Ni - 15.5Cr - 0.95 (Cb (Nb) + Ta) - 2.5Ti - 0.70Al - 7.0Fe, Consumable Electrode, Remelted or Vacuum Induction Melted, Solution Heat Treated, Precipitation-Hardenable.

This specification covers a corrosion and heat-resistant nickel alloy in the form of sheet, strip, and plate procured in inch/pound units.