Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and Rings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated.

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, wire, forgings, flash welded rings, and stock for forging, flash welded rings, or heading.