AMS 5832

Nickel Alloy, Corrosion and Heat Resistant, Welding Wire, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb(Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted

This specification covers a corrosion and heat resistant nickel alloy in the form of welding wire.