AMS 5872E

Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate, 48Ni - 20Cr - 20Co - 5.9Mo - 2.2Ti - 0.45Al, Consumable Electrode or Vacuum Induction Melted, Solution Heat Treated.

This specification covers a corrosion and heat-resistant nickel alloy in the form of sheet, strip, and plate.