AMS 5966

Nickel Alloy, Corrosion and Heat Resistant, Welding Wire 50ni 20cr 20co 5.9mo 2.2ti 0.45al Consumable Electrode Or Vacuum Induction Melted

This specification covers a corrosion and heat resistant nickel alloy in the form of welding wire.

This wire has been used typically as filler metal for gas-tungsten-ar or gas-metal-arc welding of corrosion and heat resistant nickel alloys of similar composition where the weld area is required to have strength and corrosion resistance comparable to those of the base metal, but usage is not limited to such applications.