AMS 6932

Titanium Alloy Bars, Forgings and Forging Stock 6.0Al - 4.0V Extra Low Interstitial Annealed

This specification covers a titanium alloy in the form of bars, forgings, and stock for forging.

These products have been used typically for parts requiring good weldability and ductility, combined with good notch-toughness down to -320 degrees F (-196 degrees C), but usage is not limited to such applications.

Certain processing procedures and service conditions may cause these products to become subject to stress-corrosion; SAE ARP 982 recommends practices to minimize such conditions.