ASTM A 276

This specification covers hot-finished or cold-finished bars except bars for reforging. It includes rounds, squares, and hexagons, and hot-rolled or extruded shapes, such as angles, tees, and channels in the more commonly used types of stainless steels. The bars shall be furnished in one of the following conditions: Condition A in which the bars are annealed, Condition H in which the bars are hardened and tempered at a relative temperature, Condition T in which the bars are hardened and tempered at a relatively high temperature, Condition S in which the bars are strain hardened or relatively light cold worked, and Condition B in which the bars are relatively severe cold worked. The material shall be subjected to a mechanical test to determine its tensile strength, yield strength, elongation, and Brinell hardness.