Home » Products » Stainless Steel » 304 / 304H Stainless
LITERATURE
SPECIFICATIONS
UNS: S30400, S30409
W. NR.: 1.4948
ASTM: A 240, A 959
ASME: SA 240
AMS: 5513
FEATURES
- Elevated temperature service to 1500°F
- Corrosion resistance similar to 304/304L
APPLICATIONS
- Pressure Vessels
- Petrochemical Equipment
304 / 304H
Dual certified 304 / 304H stainless is used as a material of construction up to 1500°F. Slight scaling begins at about 1200°F. This is the 0.04% minimum carbon version of type 304 stainless. It has general corrosion resistance similar to the low carbon 304/304L. However, it is subject to carbide precipitation in the heat affected zone (HAZ) of welds. Weldments may be sensitive to HAZ intergranular corrosion in oxidizing acid environments, and to polythionic acid stress corrosion cracking. The carbide precipitation is not harmful to high temperature mechanical properties.
304/304H is welded using the 22Cr 11Ni filler wire (ER308), or covered electrodes (E308). Post-weld heat treatment is not necessary for most high temperature service.
FORMS

MARKETS & INDUSTRIES
Available Forms
Available Sizes
IN-STOCK LOCATIONS
- Select a size to view
- Toledo, OH
- Cincinnati, OH
- Chicago, IL
- Houston, TX
- Los Angeles, CA
- Phoenix, AZ
- Richburg, SC
- Tampa, FL
- Tulsa, OK
- Windsor, CT