- Improved general and localized corrosion compared to 304 / 304L and 316 / 316L
- Good formability
- Good weldability
APPLICATIONS
- FGD Systems
- Chemical Process Vessels
- Condensers in Power Generation
317 / 317L
317 / 317L stainless is a molybdenum containing austenitic stainless steel, with improved corrosion resistance over 304/304L and 316/316L stainless steel. The increased levels of chromium, nickel, and molybdenum over 316L stainless steel improve chloride pitting resistance and general corrosion. Through the controlled addition of nitrogen it is common for 317L to meet the mechanical properties of 317, while maintaining a low carbon content.
FORMS


MARKETS & INDUSTRIES
Available Forms
Available Sizes
IN-STOCK LOCATIONS
- Select a size to view
- Toledo, OH
- Cincinnati, OH
- Chicago, IL
- Houston, TX
- Los Angeles, CA
- Phoenix, AZ
- Richburg, SC
- Tampa, FL
- Tulsa, OK
- Windsor, CT