Heat resistant alloy castings are available in chemistries similar, although never identical, to those of the wrought alloys. In addition there are a number of chemistries that are only available as castings. Selection of cast versus wrought will depend, among other things, upon experience, economics and delivery time.

Two key aspects to consider:

Design – Appropriate design may influence life more than the simple choice of wrought versus cast. A good design in either metal form may outlast a poor design in the other. This effect of design may or may not get factored into the user’s evaluation of his own experience.

Quality – In fabrications this usually means the welds. With castings it is internal shrinkage, porosity and residual casting stresses. Cast grids, for example, may last only a few months, or for many years, depending on the foundry source and soundness of the casting.

Cast vs Wrought Material Selection Guidelines

   Cast   Wrought   
Initial Cost   Since cast parts avoid most fabrication techniques, the price per pound of a fixture could be lower.
Pattern Cost   A pattern must be made for each different cast part design. This is fine for production runs with thousands of parts but not very economical for one or two parts at a time.
Weight   Cast parts are invariably thicker and heavier than the equivalent fabrication. This simply increases the dead weight that goes through each heat treat cycle. With radiant tubes and muffles, thicker cast walls increase fuel costs for the same volume of work heat treated. Wrought alloys are available down to nearly foil thicknesses. Thinner sections often permit weight reductions of 50% or more.
Availability & Delivery   Wrought heat resisting alloys are immediately available from stock in numerous product forms. Fabrications are quickly procured to minimize expensive downtime. When equipment is out of service, fabrications can be delivered in a couple of days to get back on-line. This is rarely true of castings.
Shapes   Certain shapes can be cast that are not commonly available hot rolled, or that cannot be fabricated economically from available wrought product forms.
Soundness   Wrought materials are normally free of the internal and external defects such as shrink and porosity that are common problems in castings.
Composition   Some alloys are available only as castings, because they lack sufficient ductility to be worked into wrought forms. This is particularly true of the very high chromium alloys.
Repairability   To repair any stainless steel or nickel alloy, the material must have retained some amount of ductility. While cast parts can fail from corrosion, the most common failure is brittle cracking making them very difficult to weld repair. Many cast alloys quickly become very brittle in service. They are unable to withstand rough handling when cold and weld repair is very difficult.
Creep Strength   Similar compositions are inherently stronger at high temperatures in the cast forms over wrought grades. This is because of the microstructure, as well as the higher carbon con-tents that are typical in a casting.
Thermal Fatigue   Thinner sections reduce the amount of internal thermal stresses within the material. This allows for inherently greater ductility in wrought materials that promote better resistance to thermal cycling and thermal shock.
Surface Finish   The smooth surface of a wrought alloy helps avoid focal points for accelerated corrosion by molten salts or carbon deposits.

The effect of a cast alloy surface and internal defects versus wrought alloy soundness on service performance is illustrated by the Rolled Alloys case history, RA330-108. The application was a grid for suspending loads in a gantry furnace at a commercial heat treat shop. The work was neutral hardening from temperatures up to 1850°F (1010°C), quenched in either molten salt, oil or brine.

When the cast HT (35%Ni 17% Cr) grid was practically new and had been exposed to only a few cycles, a particular job required increased working area for the grid. RA300 alloy plate for formed and welded to the outside of the existing cast grid.

As can be seen in the photo, the cast alloy portion suffered surface attack from soot and the quenching salt, and failed from thermal fatigue. The wrought Alloy RA330 exhibited very little surface attack and showed no fractures. The cracks in the center of the case ribs occur at the weakest spot in the cast structure.