STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Plate Thickness Variations
Plate Thickness Variation Back To All Articles Share: More Articles Quote, Buy, Track! We make it easy to get instant
Best Practices When Using Duplex Stainless Steels
Gain deeper insight into duplex stainless steel and master best practices in metallurgy for peak performance in demanding applications.
Things to Know About PREN
Highlighting the importance of factors beyond PREN, like manufacturing processes and heat treatment, is essential for predicting corrosion resistance accurately
Rolled Alloys is Coming to Tampa!
Coming to Tampa, Florida – Summer 2024 Back To All Articles Share: Quote, Buy, Track! We make it easy to
PRODEC® 17-4
PRODEC® (PRODuction EConomy), is a special quality of austenitic stainless steel. The uniformity and optimal machinability of PRODEC allows fabricators to machine at higher speeds and feeds, producing superior quality parts at the lowest total cost. It should be considered for automatic screw machines where extensive machining is required.
PRODEC 17-4 is a newly developed enhanced machining version of 17-4 stainless PH. Trials have shown PRODEC 17-4 to provide up to 30% faster machining speeds without sacrificing tool life when compared to standard 17-4. This enhanced machinability is a result of the PRODEC melting process which reduces the quantity, size, and distribution of hard oxide inclusions. As a result, improved machining properties are realized in all heat treated conditions (Condition A, H1150, H1025, etc.) PRODEC 17-4 round bar is produced in diameters ranging from 9/16″ to 6-1/2″.
17-4 is also commonly referred to as type 630 stainless. It is a martensitic, precipitation hardening stainless steel. A low temperature heat treatment can provide unusually high strength and hardness, with corrosion resistance similar to that of Type 304 austenitic stainless steel.
- Melted and processed to maximize machinability
- Improved machinability over 17-4
UNS: S17400
W. NR.: 1.4548
ASTM: A 564
ASME: SA 564
AMS: 5643
- Automatic screw machine
- Firearms production