DUPLEX STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Duplex Stainless Steels
Gain deeper insight into duplex stainless steel and master best practices in metallurgy for peak performance in demanding applications <
Things to Know About PREN
Highlighting the importance of factors beyond PREN like manufacturing processes and heat treatment is essential for predicting corrosion resistance accurately
Coming to Tampa!
We are pleased to announce the grand opening of our new bar processing facility dedicated to stainless bar processing <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
2205
2205 is a duplex (austenitic-ferritic) stainless steel containing approximately 50% ferrite and 50% aystenite in the annealed condition. 2205 has been a practical solution to chloride stress corrosion cracking problems experienced with 304/304L or 316/316L stainless. The high chromium, molybdenum and nitrogen contents provide corrosion resistance superior to 316/316L and 317/317L stainless in most environments. 2205 is not suggested for operating temperatures above 600°F
The design strength of 2205 is significantly higher than 316/316L, often permitting lighter wall construction. 2205 has good notch impact toughness down to temperatures below – 40°F. 2205 is welded with E2209 or ER2209 fillers.
- High resistance to chloride stress corrosion cracking
- Chloride pitting and crevice corrosion resistance superior to 317L stainless
- Good general corrosion resistance
- High strength
- Good sulfide stress corrosion resistance
- Useful up to 600°F
UNS: S31803, S32205
W. NR.: 1.4462
ASTM: A 240, A 276, A 479, A 789, A 790, A 182, A 923
ASME: SA 240, SA 276, SA 479, SA 789, SA 790, SA 182, SA 923
NACE: MRO175
ISO: 15156
- Chemical process vessels, piping, and heat exchangers
- FGD scrubber systems
- Pulp mill digesters, bleach washers, chip presteaming vessels
- Food process equipment
- Oil field piping
Share This Page