UNS: S66286
W. NR.: 1.4980
AMS: 5525, 5732, 5737, 5804
GE: B50T1181, B50T12, B50T81

FEATURES
  • High strength to 1000°F
  • Oxidation resistant to 1500°F
APPLICATIONS
  • Jet engine components
  • High temperature fasteners, springs
  • Non-magnetic cryogenic equipment

A-286

A-286 stainless is an age-hardenable iron base superalloy for applications requiring high strength from -320°F up to 1000°F long time, 1300-1500°F short time. Oxidation resistance is high for continuous service to 1500°F, intermittent to 1800°F. Aqueous corrosion resistance is comparable to 316/316L stainless. Heat treatment according to AMS 5525 requires a solution anneal at 1800°F, air cool. Age at 1325°F for 16 hours and then air cool.

FORMS

a286 Platea286 Round Bara286 Sheet

MARKETS & INDUSTRIES

Available Forms
Available Sizes
IN-STOCK LOCATIONS
  • Select a size to view
  • Toledo, OH
  • Cincinnati, OH
  • Chicago, IL
  • Houston, TX
  • Los Angeles, CA
  • Phoenix, AZ
  • Richburg, SC
  • Tampa, FL
  • Tulsa, OK
  • Windsor, CT
Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.