Share:

More Articles

Quote, Buy, Track!

We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!

Rolled Alloys - March Mania is Here!

NO PURCHASE NECESSARY. MANY WILL ENTER, FEW WILL WIN. Legal residents of the 50 United States (D.C.) 18 years or older. Ends 3/31/2025. Prizes are subject to change without notice. Void where prohibited.

Click for Official Rules / Printable Entry Form

VIEW FULL PRODUCT LINE
ORDER A SAMPLE

LITERATURE

Data Book
Data Sheet
Expanded Metal Information
Fabrication Information
RA 253 MA vs RA330
RA330 vs 309/310
Case Histories

SPECIFICATIONS

UNS: N08330
W. NR.: 1.4886
EN: 10095
ASTM: B 536, B 511, B 512, B 535, B 546, B 710, B 739
ASME: SB 536, SB 511, SB 535, SB 710
AMS: 5592, 5716

FEATURES
  • Oxidation resistance to 2100°F (1148°C)
  • Resistant to carburization and nitriding
  • Resistance to thermal shock
  • Good strength at elevated temperature
  • Metallurgical stability
COMMON TRADE NAMES
  • Incoloy® Alloy 330
  • Alloy 330
  • UNS N08330

ALLOY NAME

ALLOY CATEGORY

RA330® is a patented alloy designed specifically for the heat treatment industry, and to this day RA330® still outperforms the generic version made only to UNS N08330. In addition to meeting the requirements of UNS N08330, Rolled Alloys has tighter chemistry restrictions and proprietary heat treatments to produce an optimum product. Even the weld wire, RA330-04, has increased levels of manganese to avoid hot cracking. When buying a heat resistant alloy, insist on quality, insist it is RA330®.

FORMS

MARKETS & INDUSTRIES

AVAILABLE FORMS
AVAILABLE SIZES
Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.