Off-the-shelf structural shapes are typically available in 304 and 316 stainless steel. Common extruded shapes such as angles, tees, and I-beams, as well as flat bar sizes, can be found.
However, when it comes to specialty alloys, the market demand for such products is low enough that manufacturers rarely produce structural shapes for standard inventory. Limited quantities of flat or square bar are produced in a small number of alloys that are in demand for aerospace applications or where cutting from plate is prohibited. These alloys include titanium alloys and some PH stainless steels.
Flat bar production for most other stainless and nickel alloy grades is usually done only when there is a considerable demand to justify a mill production run. This run typically requires a minimum of 2500 pounds per size. However, cutting flat bar from plate can fulfill most flat bar needs, and it poses no metallurgical problems as the properties of stainless and nickel alloy plates are nearly isotropic. Although the transverse mechanical properties can be slightly lower than those in the longitudinal direction, the minimum tensile properties established for each plate material are set by testing in the transverse direction.
The main difference between a true flat bar and a flat bar cut from plate is the dimensional tolerance. In true flat bar, the width and thickness tolerances are strict and similar to those set for round bar. On the other hand, the width tolerance for cutting bar from plate is more liberal and in line with the cutting method, usually with a permitted range of variation of 1/8″. The thickness of the flat bar cut from plate is the same as that of the plate, which has tolerances skewed to the heavy side. The minimum under tolerance for plate thickness is 0.010″. However, the over tolerance is either unrestricted or is at least 0.090″ and increases with thickness.
It is important to note that when it comes to bar, edge and corner conditions can vary. For a true bar, all four sides will have a similar surface finish, whereas corners will be full and almost sharp, with only a slight break. They will also be free of any twist or camber. On the other hand, if a flat bar is cut from plate, the sides that were cut will have a different surface finish from the top and bottom, which are the original plate surfaces. Additionally, bar stripped from plate may show some twist or camber, which can vary significantly depending on the cutting method used.
Since most flat bar is cut from plate and can be deformed, at Rolled Alloys, we use a process called Gauering to straighten and condition flat bar products. The equipment used in this process is called a Gauer, named after the New Jersey based company, Gauer Metal Products, where the equipment was invented. Gauering involves passing the flat bar through the Gauer to straighten it, remove any twists, and condition the corners to ensure uniformity. This process also removes the shear burr from the corners. Flat bar cut from plate to ASTM A276 and A479 is permitted by ASTM A484.

Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements,

How the Kroll Process Produces Titanium Sponge
The Kroll process is the primary industrial method for transforming titanium ore into metallic titanium…

RA 253 MA Delivers High-Temp Performance in Industry Feature
Rolled Alloys has been featured in Heat Treat Today with the article, “A Microalloyed Solution for High-Temp Applications.”
Never Miss an Update - Subscribe Today!
Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.
Share:
QUOTE, BUY, TRACK
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements, explains how they affect material properties, and provides guidance for choosing the right alloy for any application.
How the Kroll Process Produces Titanium Sponge
The Kroll process is the primary industrial method for transforming titanium ore into metallic titanium…
RA 253 MA Delivers High-Temp Performance in Industry Feature
Rolled Alloys has been featured in Heat Treat Today with the article, “A Microalloyed Solution for High-Temp Applications.”
Welding Consumable Designations and Selection Criteria
Understanding welding consumable designations is essential for achieving strong, reliable welds. This guide breaks down AWS standards, electrode naming conventions, and key factors like polarity, base materials, and welding position to help you choose the right filler metal every time.
2025 Trade Shows
Come talk to a Rolled Alloys representative in person about your project. You can find us at these trade shows.