PIPE SIZE CHART
Nominal Pipe Size (NPS)
Nominal Pipe Size is a North American set of standards used to designate pipe diameter and thickness.
Pipe size is specified with two non-dimensional numbers: a nominal pipe size (NPS) for inside diameter based on inches, and a schedule (Sched. or Sch.) for wall thickness
PIPE SCHEDULES WALL THICKNESS (Inches)
Nominal |
O.D. Inches |
10s |
10 |
40s & Std |
40 |
80s & E.H. |
80 |
160 |
|---|---|---|---|---|---|---|---|---|
1/8" |
.405 |
.049 |
.049 |
.068 |
.068 |
.095 |
.095 |
|
1/4" |
.540 |
.065 |
.065 |
.088 |
.088 |
.119 |
.119 |
|
3/8" |
.675 |
.065 |
.065 |
.091 |
.091 |
.126 |
.126 |
|
1/2" |
.840 |
.083 |
.083 |
.109 |
.109 |
.147 |
.147 |
.187 |
3/4" |
1.050 |
.083 |
.083 |
.113 |
.113 |
.154 |
.154 |
.218 |
1" |
1.315 |
.109 |
.109 |
.133 |
.133 |
.179 |
.179 |
.250 |
1 1/4" |
1.660 |
.109 |
.109 |
.140 |
.140 |
.191 |
.191 |
.250 |
1 1/2" |
1.900 |
.109 |
.109 |
.145 |
.145 |
.200 |
.200 |
.281 |
2" |
2.375 |
.109 |
.109 |
.154 |
.154 |
.218 |
.218 |
.343 |
2 1/2" |
2.875 |
.120 |
.120 |
.203 |
.203 |
.276 |
.276 |
.375 |
3" |
3.500 |
.120 |
.120 |
.216 |
.216 |
.300 |
.300 |
.437 |
3 1/2" |
4.000 |
.120 |
.120 |
.226 |
.226 |
.318 |
.318 |
|
4" |
4.500 |
.120 |
.120 |
.237 |
.237 |
.337 |
.337 |
.531 |
4 1/2" |
5.000 |
.247 |
.355 |
|||||
5" |
5.563 |
.134 |
.134 |
.258 |
.258 |
.375 |
.375 |
.625 |
6" |
6.625 |
.134 |
.134 |
.280 |
.280 |
.432 |
.432 |
.718 |
7" |
7.625 |
.301 |
.500 |
|||||
8" |
8.625 |
.148 |
.148 |
.322 |
.322 |
.500 |
.500 |
.906 |
9" |
9.625 |
.342 |
.500 |
|||||
10" |
10.750 |
.165 |
.165 |
.365 |
.365 |
.500 |
.593 |
1.125 |
11" |
11.750 |
.375 |
.500 |
|||||
12" |
12.750 |
.180 |
.180 |
.375 |
.406 |
.500 |
.687 |
1.312 |
14" |
14.000 |
.188 |
.250 |
.375 |
.437 |
.500 |
.750 |
1.406 |
16" |
16.000 |
.188 |
.250 |
.375 |
.500 |
.500 |
.843 |
1.593 |
18" |
18.000 |
.188 |
.250 |
.375 |
.562 |
.500 |
.937 |
1.781 |
PIPE DIMENSIONS & WEIGHT
- Legend
- Wall Thickness in inches
- Steel weight in lbs. per ft.
| PIPE O.D. IN | |||||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| SIZE | INCHES | 5S | 5 | 10S | 10 | 20 | 30 | 40s & STD | 40 | 60 | 80S & E.H. | 80 | 100 | 120 | 140 | 160 | DBLE. E.H. |
| 1/8" | .405 | .035 .1383 |
.049 .1863 |
.049 .1863 |
.068 .2447 |
.068 .2447 |
.095 .3145 |
.095 .3145 |
|||||||||
| 1/4" | .540 | .049 .2570 |
.065 .3297 |
.065 .3297 |
.088 .4248 |
.088 .4248 |
.119 .5351 |
.119 .5351 |
|||||||||
| 3/8" | .675 | .049 .3276 |
.065 .4235 |
.065 .4235 |
.091 .5676 |
.091 .5676 |
.126 .7338 |
.126 .7338 |
|||||||||
| 1/2" | .840 | .065 .5383 |
.065 .5383 |
.083 .6710 |
.083 .6710 |
.109 .8510 |
.109 .8510 |
.147 1.088 |
.147 1.088 |
.187 1.304 |
.294 1.714 |
||||||
| 3/4" | 1.050 | .065 .6838 |
.065 .6838 |
.083 .8572 |
.083 .8572 |
.113 1.131 |
.113 1.131 |
.154 1.474 |
.154 1.474 |
.218 1.937 |
.308 2.441 |
||||||
| 1" | 1.315 | .065 .8678 |
.065 .8678 |
.109 1.404 |
.109 1.404 |
.133 1.679 |
.133 1.679 |
.179 2.172 |
.179 2.172 |
.250 2.844 |
.358 3.659 |
||||||
| 1 1/4" | 1.660 | .065 1.107 |
.065 1.107 |
.109 1.806 |
.109 1.806 |
.140 2.273 |
.140 2.273 |
.191 2.997 |
.191 2.997 |
.250 3.765 |
.382 5.214 |
||||||
| 1 1/2" | 1.900 | .065 1.274 |
.065 1.274 |
.109 2.085 |
.109 2.085 |
.145 2.718 |
.145 2.718 |
.200 3.631 |
.200 3.631 |
.281 4.859 |
.400 6.408 |
||||||
| 2" | 2.375 | .065 1.604 |
.065 1.604 |
.109 2.638 |
.109 2.638 |
.154 3.653 |
.154 3.653 |
.218 5.022 |
.218 5.022 |
.343 7.444 |
.436 9.029 |
||||||
| 2 1/2" | 2.875 | .083 2.475 |
.083 2.475 |
.120 3.531 |
.120 3.531 |
.203 5.793 |
.203 5.793 |
.276 7.661 |
.276 7.661 |
.375 10.01 |
.552 13.70 |
||||||
| 3" | 3.500 | .083 3.029 |
.083 3.029 |
.120 4.332 |
.120 4.332 |
.216 7.576 |
.216 7.576 |
.300 10.25 |
.300 10.25 |
.437 14.32 |
.600 18.58 |
||||||
| 3 1/2" | 4.000 | .083 3.472 |
.083 3.472 |
.120 4.973 |
.120 4.973 |
.226 9.109 |
.226 9.109 |
.318 12.51 |
.318 12.51 |
.636 22.85 |
|||||||
| 4" | 4.500 | .083 3.915 |
.083 3.915 |
.120 5.613 |
.120 5.613 |
.237 10.79 |
.237 10.79 |
.281 12.66 |
.337 14.98 |
.337 14.98 |
.437 19.01 |
.531 22.51 |
.674 27.54 |
||||
| 4 1/2" | 5.000 | .247 12.53 |
.355 17.61 |
.710 32.53 |
|||||||||||||
| 5" | 5.563 | .109 6.349 |
.109 6.349 |
.134 7.770 |
.134 7.770 |
.258 14.62 |
.258 14.62 |
.375 20.78 |
.375 20.78 |
.500 27.04 |
.625 32.96 |
.750 38.55 |
|||||
| 6" | 6.625 | .109 7.585 |
.109 7.585 |
.134 9.290 |
.134 9.290 |
.280 18.97 |
.280 18.97 |
.432 28.57 |
.432 28.57 |
.562 36.39 |
.718 45.3 |
.864 53.16 |
|||||
| 7" | 7.625 | .301 23.57 |
.500 38.05 |
.875 63.08 |
|||||||||||||
| 8" | 8.625 | .109 |
.109 |
.148 13.40 |
.148 13.40 |
.250 22.36 |
.277 24.70 |
.322 28.55 |
.322 28.55 |
.406 35.64 |
.500 43.39 |
.500 43.39 |
.593 50.87 |
.718 60.93 |
.812 67.76 |
.906 74.69 |
.885 72.42 |
| 9" | 9.625 | .342 33.9 |
.500 48.72 |
||||||||||||||
| 10" | 10.750 | .134 15.19 |
.134 15.19 |
.165 18.65 |
.165 18.65 |
.250 28.04 |
.307 34.24 |
.365 40.48 |
.365 40.48 |
.500 54.74 |
.500 54.74 |
.593 64.33 |
.718 76.93 |
.843 89.20 |
1.000 104.1 |
1.125 115.7 |
|
| 11" | 11.750 | .375 45.55 |
.500 60.07 |
||||||||||||||
| 12" | 12.750 | .156 21.07 |
.165 22.18 |
.180 24.17 |
.180 24.17 |
.250 33.38 |
.307 34.24 |
.365 40.48 |
.365 40.48 |
.500 54.74 |
.500 54.74 |
.593 64.33 |
.718 76.93 |
.843 89.20 |
1.000 104.1 |
1.125 115.7 |
|
| 14" | 14.000 | .156 23.07 |
.188 27.73 |
.250 36.71 |
.312 45.38 |
.375 54.57 |
.375 54.57 |
.437 63.37 |
.593 84.91 |
.500 72.09 |
.750 106.1 |
.937 130.7 |
1.093 150.7 |
1.250 170.2 |
1.406 189.1 |
||
| 16" | 16.000 | .165 27.90 |
.188 31.75 |
.250 42.05 |
.312 52.36 |
.375 62.58 |
.375 62.58 |
.500 82.77 |
.656 107.5 |
.500 82.77 |
.843 136.5 |
1.031 164.8 |
1.218 192.3 |
1.427 223.5 |
1.593 245.1 |
||
| 18" | 18.00 | .165 31.43 |
.188 35.76 |
.250 47.39 |
.312 59.03 |
.437 82.06 |
.375 70.59 |
.562 104.2 |
.750 138.2 |
.500 93.45 |
.937 170.8 |
1.156 208.0 |
1.375 244.1 |
1.562 274.2 |
1.781 308.5 |
||
| 20" | 20.000 | .188 39.78 |
.218 46.05 |
.250 52.73 |
.375 78.6 |
.500 104.1 |
.375 78.6 |
.593 122.9 |
.812 166.4 |
.500 104.1 |
1.031 208.9 |
1.280 256.1 |
1.500 296.4 |
1.750 341.1 |
1.968 379.0 |
||
| 22" | 22.000 | .188 43.8 |
.218 50.71 |
.250 58.07 |
.375 86.61 |
.500 114.81 |
.375 86.61 |
.875 197.41 |
.500 114.81 |
1.125 250.81 |
1.375 302.88 |
1.625 353.61 |
1.875 403.0 |
2.125 451.06 |
|||
| 24" | 24.000 | .218 55.37 |
.250 63.41 |
.250 63.41 |
.375 94.62 |
.562 140.8 |
.375 94.62 |
.687 171.2 |
.968 238.1 |
.500 125.5 |
1.218 296.4 |
1.531 367.4 |
1.812 429.4 |
2.062 483.1 |
2.344 542.13 |
||
| 26" | 26.000 | .312 85.60 |
.500 136.17 |
.375 102.63 |
.500 136.17 |
||||||||||||
| 28" | 28.000 | .312 92.26 |
.500 146.85 |
.625 182.73 |
.375 110.64 |
||||||||||||
| 30" | 30.000 | .250 79.43 |
.312 98.93 |
.312 98.93 |
.500 157.53 |
.625 196.08 |
.375 118.65 |
.500 157.53 |
|||||||||
| 32" | 32.000 | .312 105.59 |
.500 168.21 |
.625 209.43 |
.375 126.66 |
.688 230.08 |
.500 168.21 |
||||||||||
| 34" | 34.000 | .312 112.25 |
.500 178.89 |
.625 222.78 |
.375 134.667 |
.688 244.77 |
|||||||||||
| 36" | 36.000 | .312 118.92 |
.625 236.13 |
.375 142.68 |
.750 262.35 |
.500 189.57 |
|||||||||||