Nominal Pipe Sizes (NPS)
Steel pipe sizes are based on historical dimensions called Nominal Pipe Sizes (NPS) which standardize the nominal outside diameter (OD).
Additionally, a series of standard wall thicknesses known as Schedules (SCH) was also developed years ago. The units for both NPS and SCH are dimensionless. A larger number indicates a larger OD size or a heavier wall thickness. A typical description might look like 4 NPS SCH 40. In this case, this description indicates a nominal OD of 4.500” (114.3 mm) and a nominal wall thickness of 0.237” (6.02 mm). Through 8 NPS, the nominal dimensions for carbon and stainless alloy pipes are the same. In larger sizes, there are differences in some nominal wall thicknesses.
Historically, the dimensions for smaller diameter pipes were such that the inside diameter (ID) of what are now known as SCH 40 thicknesses were very close to the OD size designator. In the example above, the nominal ID is 4.026” for 4 NPS. As it became possible to make lighter (and heavier) wall thicknesses, the schedule of sizes was expanded. The sizes are standardized in ANSI B36.10 for carbon pipe and in ANSI B36.19 for stainless and nickel alloys.
Pipe tolerances will depend on the alloy and the standard to which it was produced. The general requirement standard covering most stainless pipe is ASTM/ASME A/SA 999. The OD under tolerance on all sizes is -0.031″. The over tolerance increases with OD size, but for the range of 1-1/2 to 4 NPS, the plus tolerance is also 0.031″.
This introduces the concept of ovality, where if the pipe exhibited both the maximum and minimum OD permitted, it would be out of round (oval) by 0.062”. An additional ovality allowance is permitted for thin wall pipe, which is defined as a pipe where the nominal wall is 3% or less of the OD. In such a case, the OD tolerance range applies to the mean OD, and the ovality is permitted to be 1.5% of the OD. (See Inset).
Only the minimum wall thickness is limited, which is -12.5% of the nominal wall. There is no maximum wall thickness limit. For seamless pipe, there is a limit of 10% by weight (mass) over the nominal weight. Note that this limits the average wall thickness of the seamless pipe to be no more than 10% heavy but does not limit the specific maximum wall thickness at any given point. There is no maximum thickness or weight limit for welded pipe.
Tolerances are also provided for stainless pipe on straightness (1/8” in 10’) and cut lengths (-0, +1/4”). Notice that there is no requirement or tolerance for the ID. Most nickel alloy welded pipe tolerances are identical or very similar to those for stainless. The general requirements for nickel alloy welded pipe are contained in ASTM/ASME B/SB 775. General seamless nickel alloy pipe requirements are published in ASTM/ASME B/SB 829. Because nickel alloys are more difficult to hot work, tolerances for hot-finished pipe are more generous than for stainless steel or welded and cold-finished nickel alloy products.
A comprehensive pipe size chart can be found on our website by clicking the below link.

Rolled Alloys Expands with New Phoenix, Arizona Metal Processing Facility
Rolled Alloys is opening a new 23,100-square-foot stainless bar processing facility in Phoenix, Arizona, expanding its capabilities to better serve key industries across the southwest

304 vs 316 Stainless Steel: Corrosion Resistance, Properties, & Applications
304 and 316 stainless steels are foundational materials in industrial and structural applications, valued for their durability, corrosion resistance, and versatility. While similar in performance,

Toledo Rolled Alloys Visitors Guide
Discover the future of metal processing at our state‑of‑the‑art, 250,000‑square‑foot facility in Maumee, Ohio.
Never Miss an Update - Subscribe Today!
Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.
Share:
QUOTE, BUY, TRACK
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Rolled Alloys Expands with New Phoenix, Arizona Metal Processing Facility
Rolled Alloys is opening a new 23,100-square-foot stainless bar processing facility in Phoenix, Arizona, expanding its capabilities to better serve key industries across the southwest region.
304 vs 316 Stainless Steel: Corrosion Resistance, Properties, & Applications
304 and 316 stainless steels are foundational materials in industrial and structural applications, valued for their durability, corrosion resistance, and versatility. While similar in performance, differences in chloride resistance can impact longevity, making proper grade selection key to balancing performance, cost, and service life.
Toledo Rolled Alloys Visitors Guide
Discover the future of metal processing at our state‑of‑the‑art, 250,000‑square‑foot facility in Maumee, Ohio.
Faster Order Search & Quote-To-Order Improvements
Find orders faster with a clean layout, better visibility, and direct quote-to-order functionality. Simplify your metal procurement purchasing with Rolled Alloys.
New & Expanded Product Inventory
New Titanium, Stainless, Nickel and Cobalt in Stock Now – CP Ti Grade 2, 635, 718 and More!